Zhengzhou Annec Industrial Co., Ltd.

Continuously Pushing Forward R& D of HBS for BF and Progress of Refractory Technology To Become Preferred Global Supplier in High Temperature Industry

Manufacturer from China
Verified Supplier
6 Years
Home / Products / Monolithic Refractory /

Anti Abrasion 1550C Low Cement Castable Refractory Material

Contact Now
Zhengzhou Annec Industrial Co., Ltd.
Visit Website
Province/State:henan
Country/Region:china
Contact Person:MrsHUANG
Contact Now

Anti Abrasion 1550C Low Cement Castable Refractory Material

Ask Latest Price
Video Channel
Brand Name :ANNEC
Model Number :RPJ55
Certification :ISO, CE
Place of Origin :CHINA
MOQ :1T
Price :USD 240/T
Payment Terms :L/C, T/T
Supply Ability :2000t/month
Delivery Time :5-8 working days
Packaging Details :ton bag
Color :Grey
Refractoriness :Min 1550℃
Bulk density :≥1.8g/cm3
Bending strength :≥30Mpa
Advantage 1 :Good plasticity and convenient construction
Advantage 3 :High refractoriness, up to 1650℃±50℃
Advantage 4 :Good resistance to slag intrusion
Advantage 5 :Good to spalling
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

Anti Abrasion 1550C Low Cement Castable Refractory Material

Definition:

Ceramic Anti Abrasion Castable is also called refractory clay or adhesive material (powder). It is used as a binder for refractory masonry. According to the material, it can be divided into clay, high-aluminum, silicon-magnesium refractory clay, etc.

Ceramic Anti Abrasion Castable of refractory powder, binder and impurities. Almost all refractory raw materials can be processed into powder for the preparation of refractory mud.

Ceramic Anti Abrasion Castablematerial is made of refractory clinker powder plus the appropriate amount of plastic clay as a binder and plasticizer. Its normal thermal strength is low, and the strength of the ceramic joint at high temperatures is high.

A chemically bonded refractory solution that uses hydraulic, gaseous, or thermosetting binders as a binder causes a chemical reaction and hardens before the temperature is below the temperature of the ceramic bond.

The particle size of refractory sludge varies depending on the requirements of the application. Its particle size is usually less than 1 mm, and some less than 0.5 mm or thinner.

Application:

Ceramic Anti Abrasion Castable is mainly used in coke ovens, glass furnaces, blast furnace hot air furnaces, and other industrial furnaces.


Application industries include: metallurgy, building materials, machinery, petrochemicals, glass, boilers, electricity, steel, cement, etc.

Product Description:

Ceramic Anti Abrasion Castable
Item LN-55 LN-65 LN-75
Al2O3 % ≥55 ≥65 ≥75
Refractoriness ℃ ≥1760 ≥1780 ≥1780
Cold bending strength
MPa
after dry 110℃ ≥1.0 ≥1.0 ≥1.0
after burning 1400℃X3h ≥4.0 ≥4.0 ≥4.0
Rate of permanent linear change of heating, % after burning 1400℃X3h -5~+1 -5~+1 -5~+1
Bonding time/ min 1~3 1~3 1~3
grain size/% <1.0 mm 100 100 100
>0.5 mm ≤2 ≤2 ≤2
<0.075 mm ≤50 ≤50 ≤50

Why choose us

Q: Are you trading company or manufacturer?

A: We are Manufacturer of refractory materials that have 4 plants in China; So we can provide you with high quality products at more competitive prices. we can provide you professional solutions about your problems. Although our salesman cannot reply you immediately, pls leave your email or phone number, we can let our technician directly help you ASAP.

Q: Do you accept OEM?

A: Sure, we can do OEM for much kind of brick.

Q: Is there any cost for the sample?

A: We provide free sample(Less 3 pcs) but don't bear the freight.

Q: What is the Warranty for the nortar?

A: For all the brick, we have 1 years warranty. If any quality problems on our side occurred in this period, we will take on the shipping cost and replacement.

Packaging and shipping

Standard packing: waterproof inner packing + outer packing suitable for container transportation

Anti Abrasion 1550C Low Cement Castable Refractory Material

Inquiry Cart 0